Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.80 MPa @Strain 300 % |
406 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S KE 40A-3S1727 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 2.80 MPa @Strain 100 % |
406 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F02-137D TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 2.80 MPa @Strain 0.100 %, Temperature -40.0 °C |
406 psi @Strain 0.100 %, Temperature -40.0 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 2.80 MPa @Strain 36.92 %, Temperature 120 °C |
406 psi @Strain 36.92 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.80 MPa @Strain 0.220 %, Temperature -20.0 °C |
406 psi @Strain 0.220 %, Temperature -4.00 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.80 MPa @Strain 50.0 %, Temperature 100 °C |
406 psi @Strain 50.0 %, Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |