Polymer Property : Tensile Stress = 4.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.40 MPa

@Strain 100 %,
Thickness 2.00 mm
638 psi

@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 4.40 MPa

@Strain 300 %
638 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ U 5355A-S0014 Thermoplastic Elastomer (TPE)
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Tensile Stress 4.40 MPa

@Strain 10.0 %
638 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® VT3104 TPC-ET
Extrusion Grade
Tensile Stress 4.40 MPa

@Strain 133.81 %,
Temperature 100 °C
638 psi

@Strain 133.81 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ASTM D412
ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel
Product Description: Vistamaxx 3020FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us..
Tensile Stress 4.40 MPa

@Strain 300 %
638 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel
Product Description: Vistamaxx 3020FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us..
Tensile Stress 4.40 MPa

@Strain 0.0600 %,
Temperature 180 °C
638 psi

@Strain 0.0600 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 4.40 MPa

@Strain 0.0600 %,
Temperature 60.0 °C
638 psi

@Strain 0.0600 %,
Temperature 140 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 4.40 MPa

@Strain 50.0 %
638 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® EL250 TPC-ET
Injection Molding
Tensile Stress 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® XG5855 TPC-ET
Extrusion Grade
Tensile Stress 4.40 MPa

@Strain 10.0 %
638 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 4.40 MPa

@Strain 93.62 %,
Temperature 180 °C
638 psi

@Strain 93.62 %,
Temperature 356 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers