Tensile Stress 4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE)
OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® F02-087B TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 4.20 MPa

@Strain 10.0 %
609 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PL381-H TPC-ET
Injection Molding
Tensile Stress 4.20 MPa

@Strain 2.00 %,
Time 36000 sec
609 psi

@Strain 2.00 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 4.20 MPa

@Time 3600 sec,
Strain 1.83 %
609 psi

@Time 1.00 hour,
Strain 1.83 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 4.20 MPa

@Strain 2.35 %,
Time 3.60e+6 sec
609 psi

@Strain 2.35 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 4.20 MPa

@Strain 2.52 %,
Time 3.60e+7 sec
609 psi

@Strain 2.52 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 4.20 MPa

@Strain 2.18 %,
Time 360000 sec
609 psi

@Strain 2.18 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 4.20 MPa

@Strain 10.0 %
609 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4078 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 4.20 MPa

@Strain 22.58 %,
Temperature 120 °C
609 psi

@Strain 22.58 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..