Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.2 MPa @Strain 3.25 %, Temperature 150 °C |
3800 psi @Strain 3.25 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 26.2 MPa @Strain 0.460 %, Temperature 60.0 °C |
3800 psi @Strain 0.460 %, Temperature 140 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |