Polymer Property : Tensile Stress = 38.82 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 38.82 MPa

@Strain 1.00 %,
Temperature 150 °C
5630 psi

@Strain 1.00 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided ..
Tensile Stress 38.82 MPa

@Strain 8.44 %,
Temperature 150 °C
5630 psi

@Strain 8.44 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Tensile Stress 38.82 MPa

@Strain 13.99 %,
Temperature 90.0 °C
5630 psi

@Strain 13.99 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..