Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.60 MPa @Strain 300 % |
377 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S KG 50A-3S2017 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2765 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ASTM D412 |
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Tensile Stress | 2.60 MPa @Strain 10.0 % |
377 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® XG6029 TPC-ET Extrusion Grade |
|||
Tensile Stress | 2.60 MPa @Strain 26.51 %, Temperature 120 °C |
377 psi @Strain 26.51 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.60 MPa @Strain 0.130 %, Temperature -40.0 °C |
377 psi @Strain 0.130 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 2.60 MPa @Strain 108.07 %, Temperature 90.0 °C |
377 psi @Strain 108.07 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.60 MPa @Strain 10.0 %, Temperature 23.0 °C |
377 psi @Strain 10.0 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
Tensile Stress | 2.60 MPa @Strain 6.00 %, Temperature 40.0 °C |
377 psi @Strain 6.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 2.60 MPa @Strain 11.77 %, Temperature 90.0 °C |
377 psi @Strain 11.77 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |