Polymer Property : Tensile Stress = 3520 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.27 MPa

@Strain 0.360 %,
Temperature 40.0 °C
3520 psi

@Strain 0.360 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 24.3 MPa

@Strain 8.90 %,
Temperature 90.0 °C
3520 psi

@Strain 8.90 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 24.3 MPa

@Strain 0.180 %,
Temperature -40.0 °C
3520 psi

@Strain 0.180 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 24.3 MPa

@Strain 25.7 %,
Temperature 90.0 °C
3520 psi

@Strain 25.7 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers