Mechanical Properties Metric English Comments
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature 120 °C
5080 psi

@Strain 1.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature 200 °C
5080 psi

@Strain 1.00 %,
Temperature 392 °F
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of..
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature 100 °C
5080 psi

@Strain 1.00 %,
Temperature 212 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Tensile Stress 35.0 MPa

@Strain 1.00 %
5080 psi

@Strain 1.00 %
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature -40.0 °C
5080 psi

@Strain 1.00 %,
Temperature -40.0 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature 23.0 °C
5080 psi

@Strain 1.00 %,
Temperature 73.4 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 35.0 MPa

@Strain 3.00 %,
Temperature 80.0 °C
5080 psi

@Strain 3.00 %,
Temperature 176 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 35.0 MPa

@Strain 1.00 %
5080 psi

@Strain 1.00 %
Solvay TECHNYL® B 50 H1 PA66/6, DRY
Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av..
Tensile Stress 35.0 MPa

@Strain 8.50 %,
Temperature 23.0 °C
5080 psi

@Strain 8.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Tensile Stress 35.0 MPa

@Strain 13.0 %,
Temperature 0.000 °C
5080 psi

@Strain 13.0 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..
Tensile Stress 35.0 MPa

@Strain 3.00 %,
Temperature 140 °C
5080 psi

@Strain 3.00 %,
Temperature 284 °F
ISO 527
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 35.0 MPa

@Strain 0.500 %,
Time 3600 sec
5080 psi

@Strain 0.500 %,
Time 1.00 hour
ISO 899-1
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Tensile Stress >= 35.0 MPa

@Strain 300 %
>= 5080 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 564D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress 35.0 MPa

@Strain 2.00 %,
Temperature 160 °C
5080 psi

@Strain 2.00 %,
Temperature 320 °F
ISO 527
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
Tensile Stress 35.0 MPa

@Temperature 160 °C
5080 psi

@Temperature 320 °F
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m..
Tensile Stress 35.0 MPa

@Strain 0.220 %,
Temperature 40.0 °C
5080 psi

@Strain 0.220 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..
Tensile Stress 35.0 MPa

@Strain 50.0 %
5080 psi

@Strain 50.0 %
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I
Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril..
Tensile Stress 35.0 MPa

@Strain 4.77 %,
Temperature 120 °C
5080 psi

@Strain 4.77 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Tensile Stress 35.0 MPa

@Strain 3.00 %,
Time 3.60e+6 sec
5080 psi

@Strain 3.00 %,
Time 1000 hour
140°C; DIN 50014-23/50-2
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 35.0 MPa

@Strain 2.00 %,
Time 3.60e+6 sec
5080 psi

@Strain 2.00 %,
Time 1000 hour
100°C; DIN 50014-23/50-2
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..