Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
3340 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Tensile Stress | 23.0 MPa @Strain 20.0 %, Temperature 80.0 °C |
3340 psi @Strain 20.0 %, Temperature 176 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 23.0 MPa @Strain 10.0 % |
3340 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.0 MPa @Strain 10.0 % |
3340 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 23.0 MPa @Strain 10.0 % |
3340 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 23.0 MPa @Strain 100 % |
3340 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.0 MPa @Strain 0.480 %, Temperature 40.0 °C |
3340 psi @Strain 0.480 %, Temperature 104 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | >= 23.0 MPa @Strain 300 % |
>= 3340 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 295A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 23.0 MPa @Strain 100 % |
>= 3340 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 464D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 23.0 MPa @Strain 100 % |
>= 3340 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 564D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 23.0 MPa @Strain 1.00 %, Temperature 160 °C |
3340 psi @Strain 1.00 %, Temperature 320 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Tensile Stress | >= 23.0 MPa @Strain 300 % |
>= 3340 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 23.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
3340 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |
|||
Tensile Stress | >= 23.0 MPa @Strain 300 % |
>= 3340 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 959A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |