Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 22.5 MPa @Strain 0.250 %, Temperature 40.0 °C |
3260 psi @Strain 0.250 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 22.48 MPa @Strain 2.60 %, Temperature 100 °C |
3260 psi @Strain 2.60 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 22.5 MPa @Strain 1.80 %, Temperature 0.000 °C |
3260 psi @Strain 1.80 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 22.5 MPa @Strain 0.210 %, Temperature 90.0 °C |
3260 psi @Strain 0.210 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 22.5 MPa @Strain 0.300 %, Temperature 80.0 °C |
3260 psi @Strain 0.300 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |
|||
Tensile Stress | 22.5 MPa @Strain 1.04 %, Temperature 60.0 °C |
3260 psi @Strain 1.04 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |