Mechanical Properties Metric English Comments
Tensile Stress 32.0 MPa

@Strain 12.0 %,
Temperature 160 °C
4640 psi

@Strain 12.0 %,
Temperature 320 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 32.0 MPa

@Strain 0.900 %,
Temperature -20.0 °C
4640 psi

@Strain 0.900 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 32.0 MPa

@Strain 8.50 %,
Temperature 90.0 °C
4640 psi

@Strain 8.50 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..
Tensile Stress 32.0 MPa

@Strain 2.00 %,
Temperature 23.0 °C
4640 psi

@Strain 2.00 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Tensile Stress 32.0 MPa

@Strain 4.70 %,
Temperature 90.0 °C
4640 psi

@Strain 4.70 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..
Tensile Stress 32.0 MPa

@Strain 300 %
4640 psi

@Strain 300 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 32.0 MPa

@Strain 0.600 %,
Time 3.60e+7 sec
4640 psi

@Strain 0.600 %,
Time 10000 hour
ISO 899-1
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Tensile Stress >= 32.0 MPa

@Strain 300 %
>= 4640 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 372D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 32.0 MPa

@Strain 300 %
>= 4640 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 772D PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 32.0 MPa

@Strain 300 %
>= 4640 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 598A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress 32.0 MPa

@Strain 5.60 %,
Temperature 40.0 °C
4640 psi

@Strain 5.60 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers