Mechanical Properties Metric English Comments
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Tensile Stress 2.14 MPa

@Strain 300 %,
Temperature 23.0 °C
310 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established...
Tensile Stress 2.14 MPa

@Strain 100 %
310 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.14 MPa

@Strain 300 %
310 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3845H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.14 MPa

@Strain 300 %
310 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3850H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 2.14 MPa

@Strain 300 %
310 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 2.14 MPa

@Strain 100 %
310 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 2.14 MPa

@Strain 97.14 %,
Temperature 100 °C
310 psi

@Strain 97.14 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 2.14 MPa

@Strain 97.14 %,
Temperature 100 °C
310 psi

@Strain 97.14 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers