Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 3.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.80 MPa

@Strain 100 %,
Thickness 2.00 mm
551 psi

@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 3.80 MPa

@Strain 100 %
551 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 3.80 MPa

@Strain 100 %
551 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F7870 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Stress 3.80 MPa

@Strain 5.85 %,
Temperature 0.000 °C
551 psi

@Strain 5.85 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.80 MPa

@Strain 16.33 %,
Temperature 160 °C
551 psi

@Strain 16.33 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 3.80 MPa

@Strain 71.13 %,
Temperature 150 °C
551 psi

@Strain 71.13 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 3.80 MPa

@Strain 16.33 %,
Temperature 160 °C
551 psi

@Strain 16.33 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers