Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.57 MPa @Strain 13.66 %, Temperature 120 °C |
518 psi @Strain 13.66 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.57 MPa @Strain 0.0300 %, Temperature -20.0 °C |
518 psi @Strain 0.0300 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Tensile Stress | 3.57 MPa @Strain 0.100 %, Temperature 23.0 °C |
518 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Stress | 3.57 MPa @Strain 5.00 %, Temperature 80.0 °C |
518 psi @Strain 5.00 %, Temperature 176 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 3.57 MPa @Strain 31.45 %, Temperature 100 °C |
518 psi @Strain 31.45 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |