Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 3.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.50 MPa

@Strain 100 %
508 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE)
OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 3.50 MPa

@Strain 300 %,
Temperature 23.0 °C
508 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV..
Tensile Stress 3.50 MPa

@Strain 300 %
508 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3870H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.50 MPa

@Strain 10.0 %,
Temperature 23.0 °C
508 psi

@Strain 10.0 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Tensile Stress 3.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
508 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a..
Tensile Stress >= 3.50 MPa

@Strain 100 %
>= 507 psi

@Strain 100 %
ASTM D412 Method A
Seals Eastern 7040 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 3.50 MPa

@Strain 5.00 %
508 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PB420-B TPC-ET
Blow Molding Grade
Tensile Stress 3.50 MPa

@Strain 10.0 %
508 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® XG5857 TPC-ET
Extrusion Grade
Tensile Stress 3.50 MPa

@Strain 10.0 %
508 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.50 MPa

@Strain 85.41 %,
Temperature 120 °C
508 psi

@Strain 85.41 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.50 MPa

@Strain 5.00 %
508 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 3.50 MPa

@Strain 10.0 %
508 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
Tensile Stress >= 3.50 MPa

@Strain 300 %
>= 508 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 770A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 3.50 MPa

@Strain 300 %
>= 508 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 570A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 3.50 MPa

@Strain 100 %
>= 508 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 3.50 MPa

@Strain 5.00 %
508 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EB464-01 TPC-ET
Antisqueak Blow Molding Grade
Copyright © lookpolymers.com All Rights Reserved