Polymer Property : Tensile Stress = 3.39 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.39 MPa

@Strain 300 %,
Temperature 23.0 °C
492 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish..
Tensile Stress 3.39 MPa

@Strain 300 %,
Temperature 23.0 °C
492 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi..
Tensile Stress 3.39 MPa

@Strain 23.75 %,
Temperature 90.0 °C
492 psi

@Strain 23.75 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers