Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.35 MPa @Strain 100 % |
486 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9855B TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 3.35 MPa @Strain 100 %, Temperature 21.0 °C |
486 psi @Strain 100 %, Temperature 69.8 °F |
Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Stress | 3.35 MPa @Strain 0.0700 %, Temperature 150 °C |
486 psi @Strain 0.0700 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |
|||
Tensile Stress | 3.35 MPa @Strain 5.00 %, Temperature 100 °C |
486 psi @Strain 5.00 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 3.35 MPa @Strain 5.86 %, Temperature 23.0 °C |
486 psi @Strain 5.86 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |