Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.52 MPa @Strain 0.900 %, Temperature 40.0 °C |
2686 psi @Strain 0.900 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 18.52 MPa @Strain 2.20 %, Temperature 80.0 °C |
2686 psi @Strain 2.20 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |