Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 180 MPa @Strain 2.00 %, Temperature 23.0 °C |
26100 psi @Strain 2.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Tensile Stress | 180 MPa @Strain 1.50 %, Temperature 23.0 °C |
26100 psi @Strain 1.50 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Tensile Stress | 180 MPa @Strain 2.00 %, Temperature -40.0 °C |
26100 psi @Strain 2.00 %, Temperature -40.0 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 180 MPa @Strain 3.00 %, Temperature 23.0 °C |
26100 psi @Strain 3.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 180 MPa @Strain 3.00 % |
26100 psi @Strain 3.00 % |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Stress | 180 MPa @Strain 3.00 % |
26100 psi @Strain 3.00 % |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Stress | 180 MPa @Strain 3.00 % |
26100 psi @Strain 3.00 % |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Tensile Stress | 180 MPa @Strain 2.00 %, Temperature 60.0 °C |
26100 psi @Strain 2.00 %, Temperature 140 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Stress | 180 MPa @Strain 2.00 %, Temperature 23.0 °C |
26100 psi @Strain 2.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |
|||
Tensile Stress | 180 MPa @Strain 2.00 % |
26100 psi @Strain 2.00 % |
|
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |