Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
3770 psi @Strain 5.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 26.0 MPa @Strain 100 % |
3770 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 26.0 MPa @Strain 0.600 %, Temperature 23.0 °C |
3770 psi @Strain 0.600 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Stress | 26.0 MPa @Strain 300 % |
3770 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Tensile Stress | 26.0 MPa @Strain 300 % |
3770 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 26.0 MPa @Strain 300 % |
>= 3770 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 364D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | 26.0 MPa @Strain 2.12 %, Temperature 120 °C |
3770 psi @Strain 2.12 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |