Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.93 MPa @Strain 0.200 %, Temperature 60.0 °C |
2455 psi @Strain 0.200 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |