Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.2 MPa @Strain 0.400 %, Temperature -40.0 °C |
2350 psi @Strain 0.400 %, Temperature -40.0 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 16.2 MPa @Strain 5.00 %, Temperature -30.0 °C |
2350 psi @Strain 5.00 %, Temperature -22.0 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 16.2 MPa @Strain 25.0 %, Temperature 23.0 °C |
2350 psi @Strain 25.0 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |