Polymer Property : Tensile Stress = 23.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 23.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
3340 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET  (Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
Tensile Stress 23.0 MPa

@Strain 20.0 %,
Temperature 80.0 °C
3340 psi

@Strain 20.0 %,
Temperature 176 °F
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Tensile Stress 23.0 MPa

@Strain 10.0 %
3340 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 23.0 MPa

@Strain 10.0 %
3340 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 23.0 MPa

@Strain 10.0 %
3340 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 23.0 MPa

@Strain 100 %
3340 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 23.0 MPa

@Strain 0.480 %,
Temperature 40.0 °C
3340 psi

@Strain 0.480 %,
Temperature 104 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress >= 23.0 MPa

@Strain 300 %
>= 3340 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 295A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 23.0 MPa

@Strain 100 %
>= 3340 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 464D Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 23.0 MPa

@Strain 100 %
>= 3340 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 564D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress 23.0 MPa

@Strain 1.00 %,
Temperature 160 °C
3340 psi

@Strain 1.00 %,
Temperature 320 °F
ISO 527
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
Tensile Stress >= 23.0 MPa

@Strain 300 %
>= 3340 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 23.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
3340 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
Tensile Stress >= 23.0 MPa

@Strain 300 %
>= 3340 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 959A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech