Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.44 MPa @Strain 100 %, Temperature 21.0 °C |
209 psi @Strain 100 %, Temperature 69.8 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |