Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 20.2 MPa @Strain 20.0 %, Temperature 0.000 °C |
2930 psi @Strain 20.0 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET