Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 19.5 MPa @Strain 0.600 %, Temperature 23.0 °C |
2830 psi @Strain 0.600 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Stress | 19.5 MPa @Strain 0.600 %, Temperature 23.0 °C |
2830 psi @Strain 0.600 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 19.5 MPa @Strain 5.00 %, Temperature -40.0 °C |
2830 psi @Strain 5.00 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 19.5 MPa @Strain 10.0 % |
2830 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Tensile Stress | 19.5 MPa @Strain 0.210 %, Temperature 23.0 °C |
2830 psi @Strain 0.210 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |