Mechanical Properties Metric English Comments
Tensile Stress 12.11 MPa

@Strain 0.220 %,
Temperature 150 °C
1756 psi

@Strain 0.220 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 12.11 MPa

@Strain 0.100 %,
Temperature 0.000 °C
1756 psi

@Strain 0.100 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Stress 12.11 MPa

@Strain 134.44 %,
Temperature 120 °C
1756 psi

@Strain 134.44 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers