Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.8 MPa @Strain 300 % |
1710 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6895 TPE, Extruded Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processingTypical Applications: IndustrialPackagingConsumerHeathca.. |
|||
Tensile Stress | 11.8 MPa @Strain 300 % |
1710 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3893 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 11.79 MPa @Strain 72.57 %, Temperature 120 °C |
1710 psi @Strain 72.57 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.8 MPa @Strain 0.290 %, Temperature 150 °C |
1710 psi @Strain 0.290 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |
|||
Tensile Stress | 11.8 MPa @Strain 0.100 %, Temperature 23.0 °C |
1710 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Stress | 11.8 MPa @Strain 50.0 % |
1710 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 11.8 MPa @Strain 300 % |
1710 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 11.8 MPa @Strain 300 % |
1710 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |