Polymer Property : Tensile Stress = 170 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.17 MPa

@Strain 100 %,
Temperature 23.0 °C
170 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Tensile Stress 1.17 MPa

@Strain 100 %,
Temperature 21.0 °C
170 psi

@Strain 100 %,
Temperature 69.8 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Tensile Stress 1.17 MPa

@Strain 100 %,
Temperature 23.0 °C
170 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 1.17 MPa

@Strain 100 %,
Temperature 23.0 °C
170 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
Tensile Stress 1.17 MPa

@Strain 100 %
170 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 1.17 MPa

@Strain 100 %
170 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 1.17 MPa

@Strain 0.000 %,
Temperature 60.0 °C
170 psi

@Strain 0.000 %,
Temperature 140 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 1.17 MPa

@Strain 0.000 %,
Temperature 40.0 °C
170 psi

@Strain 0.000 %,
Temperature 104 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 1.17 MPa

@Strain 0.000 %,
Temperature 90.0 °C
170 psi

@Strain 0.000 %,
Temperature 194 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Copyright © lookpolymers.com All Rights Reserved