Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 115.95 MPa @Strain 3.71 %, Temperature -20.0 °C |
16817 psi @Strain 3.71 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 115.95 MPa @Strain 0.970 %, Temperature 0.000 °C |
16817 psi @Strain 0.970 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |