Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.6 MPa @Strain 100 %, Temperature 23.0 °C |
1680 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Tensile Stress | 11.6 MPa @Strain 10.0 %, Temperature 23.0 °C |
1680 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Tensile Stress | 11.6 MPa @Strain 50.0 % |
1680 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PB420-B TPC-ET Blow Molding Grade |
|||
Tensile Stress | 11.6 MPa @Strain 100.03 %, Temperature 150 °C |
1680 psi @Strain 100.03 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Tensile Stress | 11.6 MPa @Strain 6.27 %, Temperature 150 °C |
1680 psi @Strain 6.27 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |
|||
Tensile Stress | 11.6 MPa @Strain 0.200 %, Temperature 100 °C |
1680 psi @Strain 0.200 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |