Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.1 MPa @Strain 0.150 %, Temperature 23.0 °C |
2190 psi @Strain 0.150 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |
|||
Tensile Stress | 15.1 MPa @Strain 15.0 %, Temperature 23.0 °C |
2190 psi @Strain 15.0 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 15.1 MPa @Strain 234.77 %, Temperature 120 °C |
2190 psi @Strain 234.77 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |