Mechanical Properties Metric English Comments
Tensile Stress 10.04 MPa

@Strain 0.210 %,
Temperature 90.0 °C
1456 psi

@Strain 0.210 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Tensile Stress 10.04 MPa

@Strain 0.210 %,
Temperature 90.0 °C
1456 psi

@Strain 0.210 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Tensile Stress 10.04 MPa

@Strain 60.5 %,
Temperature 100 °C
1456 psi

@Strain 60.5 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 10.04 MPa

@Strain 49.19 %,
Temperature 120 °C
1456 psi

@Strain 49.19 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved