Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.00 MPa @Strain 100 % |
145 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KA 40A-3S1767 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 1.00 MPa @Strain 100 % |
145 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3838 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.00 MPa @Strain 100 % |
145 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-2432F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 1.00 MPa @Strain 0.150 %, Temperature -40.0 °C |
145 psi @Strain 0.150 %, Temperature -40.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | >= 1.00 MPa @Strain 100 % |
>= 145 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 565A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |