Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 97.9 MPa @Strain 25.1 %, Temperature -40.0 °C |
14200 psi @Strain 25.1 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 98.2 MPa @Strain 9.00 %, Temperature -40.0 °C |
14200 psi @Strain 9.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Stress | 97.6 MPa @Strain 7.38 %, Temperature -40.0 °C |
14200 psi @Strain 7.38 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Tensile Stress | 97.7 MPa @Strain 7.00 %, Temperature -40.0 °C |
14200 psi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 97.6 MPa @Strain 7.38 %, Temperature -40.0 °C |
14200 psi @Strain 7.38 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Tensile Stress | 97.7 MPa @Strain 6.73 %, Temperature 180 °C |
14200 psi @Strain 6.73 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 98.0 MPa @Strain 0.897 %, Temperature 40.0 °C |
14200 psi @Strain 0.897 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance.. |
|||
Tensile Stress | 98.0 MPa @Strain 0.897 %, Temperature 40.0 °C |
14200 psi @Strain 0.897 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Stress | 97.7 MPa @Strain 1.38 %, Temperature 90.0 °C |
14200 psi @Strain 1.38 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Stress | 97.6 MPa @Strain 0.980 %, Temperature 23.0 °C |
14200 psi @Strain 0.980 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |
|||
Tensile Stress | 97.6 MPa @Strain 18.0 %, Temperature -40.0 °C |
14200 psi @Strain 18.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 97.8 MPa @Strain 7.00 %, Temperature -40.0 °C |
14200 psi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 98.2 MPa @Strain 8.00 %, Temperature -40.0 °C |
14200 psi @Strain 8.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 97.7 MPa @Strain 1.50 %, Temperature 0.000 °C |
14200 psi @Strain 1.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |