Mechanical Properties Metric English Comments
Tensile Stress 9.51 MPa

@Strain 0.200 %,
Temperature 100 °C
1380 psi

@Strain 0.200 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 9.51 MPa

@Strain 50.0 %
1380 psi

@Strain 50.0 %
ASTM D1708
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Tensile Stress 9.53 MPa

@Strain 14.11 %,
Temperature 60.0 °C
1380 psi

@Strain 14.11 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 9.52 MPa

@Strain 102.09 %,
Temperature 100 °C
1380 psi

@Strain 102.09 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.50 MPa

@Strain 0.800 %,
Temperature 150 °C
1380 psi

@Strain 0.800 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 9.50 MPa

@Strain 0.240 %,
Temperature 23.0 °C
1380 psi

@Strain 0.240 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..
Tensile Stress 9.51 MPa

@Strain 0.130 %,
Temperature 60.0 °C
1380 psi

@Strain 0.130 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 9.50 MPa

@Strain 42.34 %,
Temperature 150 °C
1380 psi

@Strain 42.34 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers
Tensile Stress 9.50 MPa

@Strain 6.34 %,
Temperature 40.0 °C
1380 psi

@Strain 6.34 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio..
Tensile Stress 9.52 MPa

@Strain 40.0 %,
Temperature 80.0 °C
1380 psi

@Strain 40.0 %,
Temperature 176 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 9.54 MPa

@Strain 173.66 %,
Temperature 120 °C
1380 psi

@Strain 173.66 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.53 MPa

@Strain 50.47 %,
Temperature 100 °C
1380 psi

@Strain 50.47 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 9.50 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1380 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
Tensile Stress 9.52 MPa

@Strain 88.68 %,
Temperature 60.0 °C
1380 psi

@Strain 88.68 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.54 MPa

@Strain 44.98 %,
Temperature 40.0 °C
1380 psi

@Strain 44.98 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.53 MPa

@Strain 50.47 %,
Temperature 100 °C
1380 psi

@Strain 50.47 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress >= 9.50 MPa

@Strain 300 %
>= 1380 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 585A Polyether-based TPU