Mechanical Properties Metric English Comments
Tensile Stress 9.24 MPa

@Strain 100 %
1340 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3892 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 9.22 MPa

@Strain 61.25 %,
Temperature 100 °C
1340 psi

@Strain 61.25 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.24 MPa

@Strain 108.21 %,
Temperature 90.0 °C
1340 psi

@Strain 108.21 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.23 MPa

@Strain 0.220 %,
Temperature 180 °C
1340 psi

@Strain 0.220 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 9.22 MPa

@Strain 0.700 %,
Temperature 80.0 °C
1340 psi

@Strain 0.700 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..
Tensile Stress 9.24 MPa

@Strain 0.0400 %,
Temperature 23.0 °C
1340 psi

@Strain 0.0400 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 9.25 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1340 psi

@Strain 0.100 %,
Temperature 73.4 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p..
Tensile Stress 9.22 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1340 psi

@Strain 0.100 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 9.23 MPa

@Strain 0.440 %,
Temperature 200 °C
1340 psi

@Strain 0.440 %,
Temperature 392 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 9.27 MPa

@Strain 146.52 %,
Temperature 90.0 °C
1340 psi

@Strain 146.52 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers