Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 13.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 13.93 MPa

@Strain 47.05 %,
Temperature 90.0 °C
2020 psi

@Strain 47.05 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 13.93 MPa

@Strain 0.860 %,
Temperature 90.0 °C
2020 psi

@Strain 0.860 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 13.93 MPa

@Strain 0.890 %,
Temperature 150 °C
2020 psi

@Strain 0.890 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers