Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1290 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.87 MPa

@Strain 75.25 %,
Temperature 40.0 °C
1290 psi

@Strain 75.25 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.89 MPa

@Strain 100.14 %,
Temperature 120 °C
1290 psi

@Strain 100.14 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.92 MPa

@Strain 6.99 %,
Temperature 60.0 °C
1290 psi

@Strain 6.99 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.86 MPa

@Strain 212.3 %,
Temperature 120 °C
1290 psi

@Strain 212.3 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.86 MPa

@Strain 79.22 %,
Temperature 90.0 °C
1290 psi

@Strain 79.22 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.90 MPa

@Strain 0.400 %,
Temperature 150 °C
1290 psi

@Strain 0.400 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Tensile Stress 8.88 MPa

@Strain 0.190 %,
Temperature 150 °C
1290 psi

@Strain 0.190 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Tensile Stress 8.88 MPa

@Strain 0.190 %,
Temperature 150 °C
1290 psi

@Strain 0.190 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Tensile Stress 8.89 MPa

@Strain 0.230 %,
Temperature 180 °C
1290 psi

@Strain 0.230 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Stress 8.87 MPa

@Strain 6.72 %,
Temperature 150 °C
1290 psi

@Strain 6.72 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 8.91 MPa

@Strain 50.0 %,
Temperature 100 °C
1290 psi

@Strain 50.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 8.92 MPa

@Strain 150.03 %,
Temperature 120 °C
1290 psi

@Strain 150.03 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Copyright © lookpolymers.com All Rights Reserved