Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 125 MPa @Strain 3.00 %, Temperature 23.0 °C |
18100 psi @Strain 3.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 125 MPa @Strain 4.00 %, Temperature 80.0 °C |
18100 psi @Strain 4.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 125 MPa @Strain 5.00 %, Temperature 80.0 °C |
18100 psi @Strain 5.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 125 MPa @Strain 1.00 %, Temperature 23.0 °C |
18100 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 125 MPa @Strain 2.00 %, Temperature 80.0 °C |
18100 psi @Strain 2.00 %, Temperature 176 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 125 MPa @Strain 1.00 %, Temperature 60.0 °C |
18100 psi @Strain 1.00 %, Temperature 140 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 125 MPa @Strain 3.00 %, Temperature 120 °C |
18100 psi @Strain 3.00 %, Temperature 248 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 125 MPa @Strain 1.50 %, Temperature 0.000 °C |
18100 psi @Strain 1.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 125 MPa @Strain 1.97 %, Temperature 23.0 °C |
18100 psi @Strain 1.97 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 125 MPa @Strain 0.200 %, Temperature 25.0 °C |
18100 psi @Strain 0.200 %, Temperature 77.0 °F |
|
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Tensile Stress | 125 MPa @Strain 2.00 %, Temperature 80.0 °C |
18100 psi @Strain 2.00 %, Temperature 176 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Stress | 125 MPa @Strain 4.00 %, Temperature -40.0 °C |
18100 psi @Strain 4.00 %, Temperature -40.0 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 125 MPa @Strain 1.50 %, Temperature 23.0 °C |
18100 psi @Strain 1.50 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |