Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.0 MPa @Strain 6.00 % |
12000 psi @Strain 6.00 % |
|
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Tensile Stress | 82.8 MPa @Strain 16.1 %, Temperature -20.0 °C |
12000 psi @Strain 16.1 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 82.5 MPa @Strain 28.8 %, Temperature -40.0 °C |
12000 psi @Strain 28.8 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 82.8 MPa @Strain 16.1 %, Temperature -20.0 °C |
12000 psi @Strain 16.1 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 82.4 MPa @Strain 2.03 %, Temperature 90.0 °C |
12000 psi @Strain 2.03 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Stress | 82.6 MPa @Strain 1.50 %, Temperature -40.0 °C |
12000 psi @Strain 1.50 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 82.7 MPa @Strain 2.20 %, Temperature 0.000 °C |
12000 psi @Strain 2.20 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 82.7 MPa @Strain 0.0500 % |
12000 psi @Strain 0.0500 % |
Process Temperature T2 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |