Polymer Property : Tensile Stress = 12.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 12.5 MPa

@Strain 100 %
1810 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-88-N809C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 12.5 MPa

@Strain 50.0 %
1810 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® VT3108 TPC-ET
Extrusion Grade, High Breathable, Drying of Material Required
Tensile Stress 12.5 MPa

@Strain 10.9 %,
Temperature 90.0 °C
1810 psi

@Strain 10.9 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 12.5 MPa

@Strain 10.9 %,
Temperature 90.0 °C
1810 psi

@Strain 10.9 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 12.5 MPa

@Strain 50.0 %
1810 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
Tensile Stress 12.5 MPa

@Strain 0.800 %,
Temperature 150 °C
1810 psi

@Strain 0.800 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 12.5 MPa

@Strain 0.830 %,
Temperature 90.0 °C
1810 psi

@Strain 0.830 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 12.5 MPa

@Strain 0.250 %,
Temperature 23.0 °C
1810 psi

@Strain 0.250 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers