Mechanical Properties Metric English Comments
Tensile Stress 7.90 MPa

@Strain 300 %,
Thickness 2.00 mm
1150 psi

@Strain 300 %,
Thickness 0.0787 in
Type 1, 200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 7.90 MPa

@Strain 300 %
1150 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ V 3085A-S0098 Thermoplastic Elastomer (TPE)
OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef..
Tensile Stress 7.93 MPa

@Strain 300 %
1150 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® F02-138A TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 7.93 MPa

@Strain 100 %
1150 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3991 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 7.93 MPa

@Strain 300 %
1150 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer
Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:..
Tensile Stress 7.96 MPa

@Strain 232.29 %,
Temperature 120 °C
1150 psi

@Strain 232.29 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.90 MPa

@Strain 6.00 %,
Temperature 23.0 °C
1150 psi

@Strain 6.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 7.96 MPa

@Strain 46.83 %,
Temperature 100 °C
1150 psi

@Strain 46.83 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 7.93 MPa

@Strain 3.49 %,
Temperature 0.000 °C
1150 psi

@Strain 3.49 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 7.90 MPa

@Strain 6.00 %,
Temperature 23.0 °C
1150 psi

@Strain 6.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.96 MPa

@Strain 46.83 %,
Temperature 100 °C
1150 psi

@Strain 46.83 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.93 MPa

@Strain 65.39 %,
Temperature 100 °C
1150 psi

@Strain 65.39 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 7.91 MPa

@Strain 0.330 %,
Temperature 90.0 °C
1150 psi

@Strain 0.330 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 7.92 MPa

@Strain 0.400 %,
Temperature 150 °C
1150 psi

@Strain 0.400 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Tensile Stress 7.91 MPa

@Strain 0.180 %,
Temperature 120 °C
1150 psi

@Strain 0.180 %,
Temperature 248 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 7.94 MPa

@Strain 0.110 %,
Temperature 150 °C
1150 psi

@Strain 0.110 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 7.90 MPa

@Strain 6.00 %,
Temperature 40.0 °C
1150 psi

@Strain 6.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 7.94 MPa

@Strain 100.62 %,
Temperature 120 °C
1150 psi

@Strain 100.62 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 7.91 MPa

@Strain 48.45 %,
Temperature 120 °C
1150 psi

@Strain 48.45 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 7.90 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1150 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET  (Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..
Tensile Stress 7.96 MPa

@Strain 8.44 %,
Temperature 60.0 °C
1150 psi

@Strain 8.44 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 7.91 MPa

@Strain 48.45 %,
Temperature 120 °C
1150 psi

@Strain 48.45 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers