Mechanical Properties Metric English Comments
Tensile Stress 75.6 MPa

@Strain 1.05 %,
Temperature 40.0 °C
11000 psi

@Strain 1.05 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Tensile Stress 76.1 MPa

@Strain 15.4 %,
Temperature 0.000 °C
11000 psi

@Strain 15.4 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 75.5 MPa

@Strain 9.30 %,
Temperature 0.000 °C
11000 psi

@Strain 9.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Tensile Stress 75.5 MPa

@Strain 0.420 %,
Temperature -40.0 °C
11000 psi

@Strain 0.420 %,
Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 75.9 MPa

@Strain 0.470 %,
Temperature 0.000 °C
11000 psi

@Strain 0.470 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 75.8 MPa

@Strain 4.27 %,
Temperature 150 °C
11000 psi

@Strain 4.27 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m..
Tensile Stress 75.85 MPa

@Strain 5.90 %,
Temperature 23.0 °C
11000 psi

@Strain 5.90 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 75.6 MPa

@Strain 3.40 %,
Temperature 90.0 °C
11000 psi

@Strain 3.40 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
Tensile Stress 75.8 MPa

@Strain 0.0500 %
11000 psi

@Strain 0.0500 %
Process Temperature T4
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - ..
Tensile Stress 75.8 MPa

@Strain 0.0500 %
11000 psi

@Strain 0.0500 %
Process Temperature T1
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - ..
Tensile Stress 75.6 MPa

@Strain 1.84 %,
Temperature 90.0 °C
11000 psi

@Strain 1.84 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..