Mechanical Properties Metric English Comments
Tensile Stress 11.6 MPa

@Strain 100 %,
Temperature 23.0 °C
1680 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE)
Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer..
Tensile Stress 11.6 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1680 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme..
Tensile Stress 11.6 MPa

@Strain 50.0 %
1680 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PB420-B TPC-ET
Blow Molding Grade
Tensile Stress 11.6 MPa

@Strain 100.03 %,
Temperature 150 °C
1680 psi

@Strain 100.03 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...
Tensile Stress 11.6 MPa

@Strain 6.27 %,
Temperature 150 °C
1680 psi

@Strain 6.27 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..
Tensile Stress 11.6 MPa

@Strain 0.200 %,
Temperature 100 °C
1680 psi

@Strain 0.200 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers