Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.880 MPa @Strain 0.000 %, Temperature 150 °C |
128 psi @Strain 0.000 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 0.880 MPa @Strain 0.0600 %, Temperature -20.0 °C |
128 psi @Strain 0.0600 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |