Polymer Property : Dart Drop Total Energy = 55.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 55.0 J/cm

@Temperature 0.000 °C
0.103 ft-lb/mil

@Temperature 32.0 °F
Mapal Plastics Maplon Type H Polypropylene Sheet
Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing..