Mechanical Properties Metric English Comments
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP313 Cotton Fabric
Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500"
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP315 Cotton Fabric
Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should ..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate
Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315.
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP347 Cotton Fabric
Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP615 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated ..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP680 Paper Base Laminate
Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500"
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP310U Cotton Fabric
Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0...
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP612 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP625 Paper Base Laminate
Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611.
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP321 Cotton Fabric  (discontinued **)
Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f..