Mechanical Properties Metric English Comments
Modulus of Elasticity 197 GPa

@Temperature 20.0 °C
28500 ksi

@Temperature 68.0 °F
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel
Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, ..
Modulus of Elasticity 197 GPa

@Temperature 20.0 °C
28500 ksi

@Temperature 68.0 °F
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel
Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor..