Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.34 J/cm @Thickness 3.17 mm |
15.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 8.34 J/cm @Thickness 3.17 mm |
15.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |